1.0124 (UKSt 37-2)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Quality Steel (General Structural Steels with Rm < 500 MPa) |
Chemical composition
| Standard | Fe, % | Mn, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|
| DIN 17119 | 99.223–99.8 | 0.2–0.5 | < 0.05 | < 0.17 | < 0.05 | < 0.007 |
Information on suppliers
Properties
| Property |
|---|
| Density: 7.86 g / cm3 |
Analogues
| Germany |
|---|
| UKSt 37-2 |
Standards
| Standard | Description |
|---|---|
| DIN 17119 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |