1.0208 (RSt 35-2)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Other Structural Steels (Not Intended for Heat Treatment with Rm < 500 MPa) |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
P, % |
C, % |
S, % |
N, % |
| DIN 17115 |
98.698–99.54 |
< 0.25 |
0.4–0.6 |
< 0.25 |
< 0.035 |
0.06–0.12 |
< 0.035 |
< 0.012 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7.86 G/cm3 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| N |
% |
Nitrogen |