- Main
- Brand
- Germany
- 1.4000 - 1.4999 (Stainless and Heat Resisting Steels)
- 1.4400 - 1.4499 (Stainless Steel with Ni > = 2.5% with Mo but without Nb and Ti)
1.4468 (GX2CrNiMoN25-6-3)
Classification
Chemical composition
Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % | N, % |
---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % | N, % |
EN 10283 | 59.16–67.38 | < 1 | < 2 | 24.5–26.5 | < 0.5 | 5.5–7 | < 0.035 | < 0.03 | < 0.025 | 2.5–3.5 | 0.12–0.25 |
Information on suppliers
Physical characteristics
Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ |
---|---|---|---|---|
Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ |
20 | 15 | 7700 | 0.45 | |
100 | 13 | |||
300 | 14 |
Mechanical properties at 20 °C
Analogues
Standards
Standard | Description |
---|---|
Standard | Description |
EN 10283 | |
DIN EN 10283:2010 | |
DIN EN 10283:2019 | |
DIN EN 10340-2:2017 | |
DIN EN 10340-2:2019 |
Description of chemical elements
Description of physical characteristics
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
$$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
$$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
$$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
$$c\cdot 10^{-3}$$ | $$\frac{J}{kg\cdot K}$$ | The specific heat of the material (range 20°C–T) |
Description of mechanical properties
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
$$\sigma_{0.2}$$ | $$MPa$$ | Tensile stress required to produce a total elongation of 0.2% |
$$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
$$\epsilon_L$$ | % | Elongation at break (longitudinal) |
$$KV_{L}$$ | $$J$$ | Impact energy (longitudinal) |