01H25tBYU-VI (CS76-VI)
It is used for the production of equipment for welding, evaporation devices (for the production of sodium sulphide, caustic soda and other types of chemical reagents). Used as a welding material — provides welded joints with high ductility and toughness.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % | Nb, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-3547-83 | 71.399–75.7 | < 0.5 | < 0.001 | < 0.7 | 24–26 | 0.1–0.3 | < 0.15 | < 0.4 | 0.1–0.2 | < 0.015 | < 0.01 | < 0.015 | 0.1–0.3 | < 0.01 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 7600 |
Wärmebehandlungsmodi
| Verarbeitung |
|---|
| Aushärten von 850-900 ° C in Wasser. |
Standards
| Standard | Description |
|---|---|
| TU 14-1-3547-83 | TU 14-1-3547-83 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| N | % | Nitrogen |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |