Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % | W, % |
GOST 5632-14 | 33.605–47.55 | < 0.6 | < 0.005 | < 1.5 | < 0.2 | 19–22 | < 0.2 | < 0.25 | 25–30 | < 0.1 | < 0.3 | < 0.02 | < 0.1 | < 0.02 | 0.7–1.3 | 2.8–3.5 | 0.15–0.3 | 4.8–6 |
Standard | Description |
---|---|
Standard | Description |
GOST 5632-14 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |