Alloy 33NKGD
No foreign analogues
It is used for the manufacture of vacuum junctions with glasses P-6, C72−4; TKLR * 1,000,000 in the temperature range from -60 to +400 ºC no more than 7.0−7.8
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With given TCLE |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 60.21–63.6 | < 0.2 | 0.4–0.8 | 3.2–4.2 | 0.8–1 | 32–33.5 | < 0.02 | < 0.05 | < 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | Cp, Дж/кг·К |
|---|---|---|---|---|
| 20 | 13–16 | 60–70 | 8220 | 450 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Tape | GOST 10994-74 | 100 | Transverse | 400–450 | 200–240 | 25–50 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Tape | GOST 10994-74 | 140–170 |
Limit operating modes
| Standard | Температура, °C |
|---|---|
| GOST 10994-74 | < 350 |
Wärmebehandlungsmodi
| Verarbeitung |
|---|
| Glühen |
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| Cp | Дж/кг·К | Specific heat of material |
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |