38HNM
production of tubular billet for the manufacture of seamless pipes.
production of tubular billet for the manufacture of seamless pipes.
Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
OST 14-21 - 77 | 96.065–97.95 | 0.17–0.37 | 0.75–1.05 | 0.4–0.7 | < 0.3 | 0.4–0.7 | < 0.045 | 0.33–0.43 | < 0.04 | < 0.3 |
Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | d5, % | Treatment |
---|---|---|---|---|---|---|---|---|---|---|
Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | d5, % | Treatment |
Pipe billet | OST 14-21 - 77 | Ø 80 | 750 | 550 | 40 | 500 | 12 | Normalized and tempered |
Standard | Description |
---|---|
Standard | Description |
OST 14-21 - 77 |
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
d5 | % | Elongation at break |
$$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
$$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
$$\psi$$ | % | Reduction in cross section on fracture |
$$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |