Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | P, % | C, % | S, % | Nb, % | Y, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | P, % | C, % | S, % | Nb, % | Y, % | Mo, % | W, % |
TU 5.961-111512-93 | 40.67–47.75 | 1.4–1.7 | < 0.005 | < 0.05 | 0.8–1.1 | 24–26 | 0.1–0.2 | < 0.2 | 24–27 | < 0.1 | < 0.1 | < 0.015 | 0.35–0.45 | < 0.01 | 1–1.3 | < 0.1 | 0.2–0.4 | 0.4–0.6 |
Standard | Description |
---|---|
Standard | Description |
TU 5.961-111512-93 | TU 5.961-111512-93 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mg | % | Magnesium |
Mn | % | Manganese |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
Zr | % | Zirconium |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Y | % | Yttrium |
Mo | % | Molybdenum |
W | % | Tungsten |
Do not trust the content. The original aloro.org.