σU
MPa
ϵL

999

high purity aluminum

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Primary aluminum

Chemical composition

Standard Al, %
GOST 11069-2001 < 99.999

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers \sigma _{U}σU, MPaMPa \epsilon_LϵL, % Treatment
Alloy Cast 50 45

Brinell hardness number

Rolling Standard Classifiers Value, HBW
Alloy Cast 13–15

Standards

Standard Description
GOST 11069-2001 GOST 11069 - 2001

Description of chemical elements

Element Units of measurement Description
Al % Aluminium

Description of mechanical properties

Parameter Units of measurement Description
\sigma _{U}σU MPaMPa Ultimate tensile strength
\epsilon_LϵL % Elongation at break (longitudinal)