Alloy aluminum AL29 (AMg7)

Chemical composition

  • Al Aluminum Rest
    Be Beryllium <0.01
    Fe Iron <0.9
    Si Silicon 0.5 — 1.0
    Mg Magnesium 6.0 — 8.0
    Mn Manganese 0.25 — 0.60
    Cu Copper <0.1
    Zn Zinc <0.2
    Ot Total impurities <1.0
    Analogs in Russia
  • AMg7 GOST 1583−93

    AL29 GOST 1583−93

    AMg7 GOST R 55375−12

    AL29 GOST R 55375−12

    AMg7 GOST R 55375−12

    AL29 GOST R 55375−12

For the manufacture of shaped castings. technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST 2685−75 Cast aluminum alloys. GOST R 55375−12 grades Primary aluminum and alloys based on it. GOST R 55375−12 grades Primary aluminum and alloys based on it. Stamps

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Chemical composition

Standard Fe, % Si, % Mg, % Mn, % Cu, % Zn, % Al, %
GOST 1583-93 < 1 0.5–1 6–8 0.25–0.6 < 0.1 < 0.2 89.4–93.25

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers \sigma _{U}, MPa \epsilon_L, % Treatment
210 3 injection molding

Brinell hardness number

Rolling Standard Classifiers Value, HBW
Casting in sandy form 60

Analogues

USA
A535.0

Standards

Standard Description
GOST 1583-93

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mg % Magnesium
Mn % Manganese
Cu % Copper
Zn % Zinc
Al % Aluminium

Description of mechanical properties

Parameter Units of measurement Description
\sigma _{U} MPa Ultimate tensile strength