BB751P
For the manufacture of heat-resistant products of a responsible purpose
For the manufacture of heat-resistant products of a responsible purpose
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | V, % | Al, % | Pb, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | V, % | Al, % | Pb, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % |
GOST 52802-2007 | < 1 | < 0.3 | < 0.015 | < 0.01 | < 0.3 | 14–16 | 10–12 | 2.5–3.1 | 50.09–59.86 | 0.4–0.8 | 3.7–4.2 | < 0.07 | < 0.01 | < 0.015 | 0.04–0.08 | < 0.009 | 3–3.5 | < 0.02 | 4–5 | 2.5–3.5 |
Standard | Description |
---|---|
Standard | Description |
GOST 52802-2007 | GOST |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mg | % | Magnesium |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
Pb | % | Lead |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
La | % | Lanthanum |
Mo | % | Molybdenum |
W | % | Tungsten |
Do not trust the content. The original aloro.org.