BrO6S6Ts3

for the manufacture of steam and water valves

Classification

Country Section Category
CIS, Russia, Ukraine Bronze Tin cast bronze

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers \sigma _{U}, MPa \sigma_{Y}, MPa \sigma_{0.5}, MPa \psi, % KCU\cdot 10^{3}, \frac{J}{m^2} Treatment
Casting in sandy form 145–195 8–12 225
Casting in chill mold 175–215 80–195 4–8 8 294

Brinell hardness number

Rolling Standard Classifiers Value, HBW
Casting in chill mold 64–73.5
Casting in sandy form 59

Coefficients of Friction

coefficient of friction with lubrication coefficient of friction without lubrication
0.009 0.16

Standards

Standard Description
GOST 613-79

Description of mechanical properties

Parameter Units of measurement Description
\sigma_{Y} MPa Yield strength
\sigma_{0.5} MPa Tensile stress required to produce a total elongation of 0.5%
\sigma _{U} MPa Ultimate tensile strength
\psi % Reduction in cross section on fracture
KCU\cdot 10^{3} \frac{J}{m^2} Impact toughness