CS108 (02Х25Н22АМ2)
Classification
Chemical composition
Note: Electroslag remelting (-Sh): S <0.015
Note: Nuclear industry: Cu <0.30
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Cr, % | Ti, % | Ni, % | Sb, % | V, % | Pb, % | As, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Cr, % | Ti, % | Ni, % | Sb, % | V, % | Pb, % | As, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % | W, % |
GOST 5632-14 | 45.236–51.4 | < 0.4 | < 0.005 | < 0.001 | < 0.001 | 1.5–2 | 24–26 | < 0.2 | 21–23 | < 0.005 | < 0.2 | < 0.001 | < 0.005 | < 0.001 | < 0.02 | < 0.02 | < 0.015 | < 0.05 | 2–2.5 | 0.1–0.14 | < 0.2 |
Note: Electroslag remelting (-Sh): S <0.015
Note: Nuclear industry: Cu <0.30
Standard | Description |
---|---|
Standard | Description |
GOST 5632-14 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Ca | % | Calcium |
Mn | % | Manganese |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
Sb | % | Antimony |
V | % | Vanadium |
Pb | % | Lead |
As | % | Arsenic |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |
Do not trust the content. The original aloro.org.