ChS70U-VI
Classification
Chemical composition
Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | Zr, % | Al, % | Pb, % | P, % | C, % | S, % | Nb, % | Y, % | Mo, % | N, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | Zr, % | Al, % | Pb, % | P, % | C, % | S, % | Nb, % | Y, % | Mo, % | N, % | W, % |
TU 1-801-223-96 | < 0.5 | < 0.3 | 0.02 | < 0.0005 | < 0.3 | 10–11.5 | 15–16 | 4.2–4.8 | < 0.07 | 54.5595–61.62 | < 0.003 | 0.05 | 2.8–3.2 | < 0.001 | < 0.008 | 0.06–0.12 | < 0.008 | 0.1–0.3 | 0.05 | 1.6–2.3 | < 0.01 | 4.5–5.9 |
Information on suppliers
Standards
Standard | Description |
---|---|
Standard | Description |
TU 1-801-223-96 |
Description of chemical elements
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Bi | % | Bismuth |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
Sb | % | Antimony |
Zr | % | Zirconium |
Al | % | Aluminium |
Pb | % | Lead |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Y | % | Yttrium |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |