EI325
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| 96.24–97.65 | 0.6–1 | 0.15–0.4 | 1–1.3 | < 0.3 | < 0.03 | 0.6–0.7 | < 0.03 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Berechnete Eigenschaften Dichte: 7,78 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |