EI444 (XH72MTU)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 4 | < 1 | < 0.6 | 19–22 | 2–3 | < 0.5 | 63.14–75 | < 0.6 | < 0.03 | < 0.1 | < 0.03 | 4–5 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Berechnete Eigenschaften Dichte: 8,38 g / cm3 |