EI468
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| 61.095–68.1 | < 1 | 5.5–7 | 14–16 | 0.4–0.7 | 12–14 | < 0.055 | < 0.12 | < 0.03 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Berechnete Eigenschaften Dichte: 7,81 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |