EI5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| 91.97–93.1 | 0.1–0.15 | 0.5–0.6 | 0.25–0.5 | 4.5–4.9 | < 0.03 | 0.35–0.42 | < 0.03 | 1.2–1.4 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Berechnete Eigenschaften Dichte: 7,92 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |