EI676 (52H)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| 45.91–49 | < 0.2 | < 0.5 | < 0.3 | 49.91–54.09 | < 0.02 | < 0.05 | < 0.02 |
Information on suppliers
Properties
| Property |
|---|
| Calculated properties Density: 8.4 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |