Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Nb, % | La, % | Y, % | Mo, % | W, % | Hf, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Nb, % | La, % | Y, % | Mo, % | W, % | Hf, % |
TU 14-1-4026-85 | < 3 | < 0.4 | 0.01 | < 0.5 | 5–6 | 14.5–16 | 1.5–2.3 | 56.35–67.88 | 1.5–2.3 | < 0.015 | < 0.005 | < 0.01 | 1.5–2 | 0.02 | 0.05 | 3.5–5 | 4.5–6 | 0.04 |
Standard | Description |
---|---|
Standard | Description |
TU 14-1-4026-85 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
La | % | Lanthanum |
Y | % | Yttrium |
Mo | % | Molybdenum |
W | % | Tungsten |
Hf | % | Hafnium |