Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | La, % | Y, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | La, % | Y, % | W, % |
TU 14-1-3182-81 | 11–13 | < 0.5 | 0.009 | < 0.4 | 6–7 | 16–18 | 2.5–3 | < 0.07 | 41.889–51.751 | < 0.02 | 1.3–1.8 | < 0.015 | < 0.05 | < 0.007 | 1.4–1.7 | 0.02 | 0.02 | 10–12.5 |
Standard | Description |
---|---|
Standard | Description |
TU 14-1-3182-81 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
La | % | Lanthanum |
Y | % | Yttrium |
W | % | Tungsten |