HN33KVYu (EK102)
Classification
Chemical composition
Note: Nd or La
Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Nd, % | La, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Nd, % | La, % | Mo, % | W, % |
GOST 5632-14 | < 3 | < 0.8 | < 0.5 | 26–30 | 20–23 | < 0.2 | < 0.07 | 24.704–40.69 | < 0.2 | 0.3–0.7 | < 0.013 | 0.01–0.1 | < 0.013 | < 0.2 | < 0.1 | < 0.1 | < 0.3 | 13–16 |
Note: Nd or La
Standard | Description |
---|---|
Standard | Description |
GOST 5632-14 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Nd | % | Neodymium |
La | % | Lanthanum |
Mo | % | Molybdenum |
W | % | Tungsten |