HN52KVMTYUB (EP975P)
Classification
Chemical composition
Note: Allowed: Ti + 0.1, Al +0.2, W - 0.5
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % | Hf, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % | Hf, % |
GOST Р 52802-07 | < 0.5 | < 0.5 | < 0.02 | < 0.02 | < 0.5 | 10–12 | 8–10 | 1.6–2.2 | 52.576–61.56 | < 0.05 | 5–5.4 | < 0.02 | < 0.015 | 0.04–0.08 | < 0.009 | 1.8–2.2 | < 0.01 | 2.4–3.2 | 9.1–9.8 | 0.5–0.9 |
Note: Allowed: Ti + 0.1, Al +0.2, W - 0.5
Standard | Description |
---|---|
Standard | Description |
GOST Р 52802-07 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mg | % | Magnesium |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
Zr | % | Zirconium |
Al | % | Aluminium |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
La | % | Lanthanum |
Mo | % | Molybdenum |
W | % | Tungsten |
Hf | % | Hafnium |