Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
GOST 5632-14 | < 4 | < 0.4 | < 0.008 | < 0.5 | < 0.2 | 17.5–20 | 1–1.4 | < 0.07 | 57.062–70.05 | < 0.2 | 1.9–2.3 | < 0.03 | < 0.015 | 0.05–0.1 | < 0.015 | < 0.2 | 4–6 | 5.5–7.5 |
Standard | Description |
---|---|
Standard | Description |
GOST 5632-14 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
W | % | Tungsten |
Do not trust the content. The original aloro.org.