XH66VMTYUB (EI698MP, VZh136)
Classification
Chemical composition
Note: Allowed: Al + 0.1
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
GOST Р 52802-07 | < 1.5 | < 0.45 | < 0.005 | < 0.03 | < 0.4 | 15.5–17.5 | 0.8–1.2 | 66.438–74.1 | 0.8–1.5 | < 0.005 | 2–2.4 | < 0.01 | < 0.015 | < 0.04 | < 0.007 | 2.2–2.6 | 3.8–4.4 | 0.8–1.5 |
Note: Allowed: Al + 0.1
Standard | Description |
---|---|
Standard | Description |
GOST Р 52802-07 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mg | % | Magnesium |
Mn | % | Manganese |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
V | % | Vanadium |
Zr | % | Zirconium |
Al | % | Aluminium |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
W | % | Tungsten |
Do not trust the content. The original aloro.org.