MC (molybdenum)
Making wire intended for manufacturing electronic devices and light sources
Making wire intended for manufacturing electronic devices and light sources
Standard | Si, % | Mo, % |
---|---|---|
Standard | Si, % | Mo, % |
GOST 27266-87 | 0.019–0.04 | < 99.92 |
Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
---|---|---|---|---|---|
Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
20 | 4.9 | 138 | 10.22 | 0.256 | 0.085 |
Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
---|---|---|---|---|---|---|
Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
Wire | GOST 27266-87 | 1186 |
Standard | Description |
---|---|
Standard | Description |
GOST 27266-87 |
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
$$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
$$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
$$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
$$c\cdot 10^{-3}$$ | $$\frac{J}{kg\cdot K}$$ | The specific heat of the material (range 20°C–T) |
$$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |