NBP-b
The niobium powder for capacitors, alloying and other purposes
The niobium powder for capacitors, alloying and other purposes
Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Co, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | C, % | O, % | Nb, % | Mo, % | N, % | W, % | H, % | Ta, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Co, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | C, % | O, % | Nb, % | Mo, % | N, % | W, % | H, % | Ta, % |
GOST 26252-84 | < 0.003 | < 0.003 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.003 | < 0.001 | < 0.001 | < 0.002 | < 0.01 | < 0.2 | > 99.632 | < 0.005 | < 0.02 | < 0.005 | < 0.01 | < 0.1 |
Standard | Description |
---|---|
Standard | Description |
GOST 26252-84 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Mn | % | Manganese |
Co | % | Cobalt |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
Zr | % | Zirconium |
Al | % | Aluminium |
C | % | Carbon |
O | % | Oxygen |
Nb | % | Niobium |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |
H | % | Hydrogen |
Ta | % | Tantalum |