Niobium alloy
Classification
Chemical composition
Note: Ulba Metallurgical Plant
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | P, % | C, % | O, % | Nb, % | Mo, % | N, % | W, % | H, % | Ta, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | P, % | C, % | O, % | Nb, % | Mo, % | N, % | W, % | H, % | Ta, % |
< 0.003 | < 0.003 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.02 | < 0.01 | < 0.01 | > 99.814 | < 0.002 | < 0.01 | < 0.005 | < 0.001 | < 0.1 |
Note: Ulba Metallurgical Plant
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Ca | % | Calcium |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
Zr | % | Zirconium |
Al | % | Aluminium |
P | % | Phosphorus |
C | % | Carbon |
O | % | Oxygen |
Nb | % | Niobium |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |
H | % | Hydrogen |
Ta | % | Tantalum |