NK0.2Ev
Classification
Chemical composition
Note: Ni: Ni + Co
Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % |
GOST 19241-16 | < 0.07 | 0.15–0.25 | < 0.001 | < 0.05 | < 0.001 | < 0.04 | < 0.1 | < 0.04 | < 0.002 | 99.378–99.85 | < 0.001 | < 0.01 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.05 | < 0.003 |
Note: Ni: Ni + Co
Standard | Description |
---|---|
Standard | Description |
GOST 19241-16 | |
GOST 19241-80 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Bi | % | Bismuth |
Mn | % | Manganese |
Co | % | Cobalt |
Cu | % | Copper |
Zn | % | Zinc |
Ni | % | Nickel |
Sb | % | Antimony |
Al | % | Aluminium |
Pb | % | Lead |
As | % | Arsenic |
Cd | % | Cadmium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Do not trust the content. The original aloro.org.