Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Ca, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Ca, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % |
GOST 9722-97 | < 0.002 | < 0.001 | < 0.0003 | < 0.001 | < 0.0003 | < 0.005 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | > 99.7025 | < 0.0003 | < 0.0003 | < 0.001 | < 0.0003 | < 0.001 | < 0.28 | < 0.001 |
Standard | Description |
---|---|
Standard | Description |
GOST 9722-97 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Bi | % | Bismuth |
Ca | % | Calcium |
Mn | % | Manganese |
Co | % | Cobalt |
Cu | % | Copper |
Zn | % | Zinc |
Ni | % | Nickel |
Sb | % | Antimony |
Pb | % | Lead |
As | % | Arsenic |
Cd | % | Cadmium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |