Sv-02H15N65M13V3TYu (EP642)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-1914-76 |
< 4 |
< 0.35 |
< 0.6 |
14–16 |
1.3–1.6 |
58.47–70.1 |
0.6–0.9 |
< 0.02 |
< 0.01 |
< 0.04 |
< 0.01 |
12–14 |
2–4 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 8.97 G/cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |