Sv-03X12N8G3M2 (ChS48)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Zr, % |
P, % |
C, % |
S, % |
Y, % |
Mo, % |
Ta, % |
| TU 14-1-2646-79 |
71.545–77.2 |
< 0.2 |
2.4–3.4 |
11–13 |
0.1 |
< 0.4 |
7–8.5 |
0.1 |
< 0.015 |
< 0.03 |
< 0.01 |
0.1 |
2–2.5 |
0.1 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7.91 G/cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Y |
% |
Yttrium |
| Mo |
% |
Molybdenum |
| Ta |
% |
Tantalum |