Sv-03H15N35G7M6B
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-2143-77 |
30.83–38.6 |
< 0.3 |
6–7.5 |
14–16 |
34–36 |
< 0.02 |
< 0.03 |
< 0.02 |
1.4–1.8 |
6–7.5 |
Information on suppliers
Свойства
| Свойство |
| Плотность: 8.26 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |