Sv-03H20N70G3B3TU
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 2 | < 0.2 | 2.8–4 | < 0.05 | 19–22 | 0.2–0.8 | < 0.3 | 67.54–75.8 | < 0.015 | < 0.03 | < 0.015 | 2.2–2.8 | < 0.25 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Dichte: 8.45 G/cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |