Sv-04X19H5AG12M (EP568)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
|
57.992–64.3 |
0.2–0.7 |
11.5–13.5 |
18–20 |
4.5–5.5 |
< 0.2 |
< 0.03 |
< 0.06 |
< 0.018 |
1.2–1.6 |
0.3–0.4 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Sv-04X19H5AG12M |
Analogues
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |