Sv-04X20H10G2BU
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| OST 24.300.04-91 |
65.377–70.6 |
< 0.3 |
1.6–2.2 |
18–20 |
9–10.5 |
< 0.018 |
< 0.04 |
< 0.015 |
0.8–1.3 |
< 0.25 |
Note: Weld metal
Note: Argon arc welding
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7,83 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |