Sv-05X15H9G6AM (ChS31)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| OST 26-291-94 |
64.99–69.48 |
< 0.4 |
5.5–7 |
14.5–15.5 |
9–10 |
< 0.02 |
< 0.05 |
< 0.02 |
1.4–1.8 |
0.12–0.22 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7,85 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |