Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ti, % Ni, % V, % Al, % As, % P, % C, % S, % Mo, % N, %
TU 1200-053-00187240-2010 96.846–98.4 0.2–0.4 0.9–1.3 < 0.3 < 0.04 < 0.2 < 0.05 < 0.05 < 0.04 < 0.012 < 0.09 < 0.01 0.5–0.65 < 0.012

Note: N> 0.010 - as agreed

Information on suppliers

Eigenschaften

Eigenschaft
Gemäß TU 1200-053-00187240-2010 Temporärer Widerstand: 588 - 784 MPa
Dichte: 7,86 g / cm³

Standards

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Ti % Titan
Ni % Nickel
V % Vanadium
Al % Aluminium
As % Arsenic
P % Phosphorus
C % Carbon
S % Sulfur
Mo % Molybdenum
N % Nitrogen