Sv-08H15N23V7G7M2 (EP88)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-4981-91 |
39.495–50 |
< 0.35 |
6–8 |
14–16 |
22–25 |
< 0.035 |
< 0.1 |
< 0.02 |
2–3 |
6–8 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Gemäß TU 14-1-4981-91 Hinweis Die mechanischen Eigenschaften sind nicht standardisiert |
| Dichte: 8,83 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |