Sv-08X15H5D2TU-Sh
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
| TU 14-1-997-2012 |
74.212–79.92 |
< 0.7 |
< 1 |
13.5–14.8 |
0.03–0.15 |
1.75–2.5 |
4.8–5.8 |
< 0.02 |
< 0.8 |
< 0.018 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Gemäß TU 14-1-997-2012 Hinweis Mechanische Eigenschaften sind nicht standardisiert Mechanische Eigenschaften: wie vereinbart |
| Dichte: 7,78 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |