Sv-08H20N57M8V8T3R-ID (EP533-ID)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-2048-77 |
< 3 |
< 0.3 |
< 0.005 |
< 0.5 |
> 19 |
2.3–2.9 |
55.77–64.7 |
< 0.4 |
< 0.015 |
< 0.1 |
< 0.01 |
7–9 |
7–9 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 9,31 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |