Sv-10GAA
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cr, % |
Ni, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU 1200-053-00187240-2010 |
97.466–98.625 |
< 0.06 |
< 0.08 |
1.1–1.3 |
< 0.2 |
< 0.3 |
0.015–0.035 |
< 0.08 |
< 0.012 |
0.06–0.1 |
< 0.005 |
0.2–0.35 |
< 0.012 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Temporärer Widerstand: 700 - 900 MPa |
| Dichte: 7,87 g / cm³ |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |