Sv-10X22H7SAT (EP704)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Foundry aluminum alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
N, % |
| TU 14-1-3030-80 |
66.585–71.5 |
0.6–1 |
1–1.6 |
20–22 |
0.4–0.8 |
6.5–7.8 |
< 0.02 |
< 0.1 |
< 0.025 |
< 0.07 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Berechnete Eigenschaften Dichte: 7,72 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| N |
% |
Nitrogen |