Sv-10N3GMT (10N3GMT)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-1392-75 |
94.615–96.15 |
< 0.3 |
1.1–1.4 |
< 0.2 |
0.05–0.12 |
2.5–2.8 |
< 0.025 |
< 0.12 |
< 0.02 |
0.2–0.4 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7,88 g / cm³ |