Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-997-2012 |
81.815–85.88 |
< 0.6 |
< 0.6 |
10.5–12 |
< 0.2 |
1.5–1.8 |
0.18–0.3 |
< 0.03 |
0.09–0.13 |
< 0.025 |
0.25–0.5 |
1.6–2 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Gemäß TU 14-1-997-2012 Hinweis Mechanische Eigenschaften sind nicht standardisiert Mechanische Eigenschaften: wie vereinbart |
| Berechnete Eigenschaften Dichte: 7,99 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |