Sv-12X17G9AN4
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
N, % |
| TU 14-1-997-74 |
65.575–72.35 |
< 0.8 |
8–10.5 |
16–18 |
< 0.2 |
3.5–4.5 |
< 0.035 |
< 0.12 |
< 0.02 |
0.15–0.25 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Gemäß TU 14-1-997-74 Hinweis Nicht geregelt |
| Berechnete Eigenschaften Dichte: 7,7 g / cm3 |
Analogues
| USA |
Germany |
| S20200 |
X12CrMnNiN17-7-5 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| N |
% |
Nitrogen |