St-13H25N18 (H-72)
Welding wire cold drawn alloy steel welding (surfacing), and the manufacture of electrodes
Welding wire cold drawn alloy steel welding (surfacing), and the manufacture of electrodes
Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
---|---|---|---|---|---|---|---|---|
GOST 2246-70 | 50.81–58 | < 0.5 | 1–2 | 24–26.5 | 17–20 | < 0.025 | < 0.15 | < 0.015 |
Property |
---|
Wire according to GOST 2246 Note Fluctuations in the tensile strength in one coil of wire with a diameter of more than 1.4 mm should not exceed 90 N / mm2. |
For welding Diameter: 0.3 - 0.5 mm; Temporary resistance: 890 - 1390 MPa |
Diameter: 0.8 - 1.5 mm; Temporary resistance: 890 - 1340 MPa |
Diameter: 1.6mm; Temporary resistance: 890 - 1290 MPa |
Diameter: 2mm; Temporary resistance: 790 - 1190 MPa |
Diameter:> 2 mm; Temporary resistance: 690 - 1040 MPa |
For the manufacture of electrodes Diameter: 1.6 mm; Temporary resistance: 690 - 990 MPa |
Diameter: 2mm; Temporary resistance: 690 - 990 MPa |
Diameter:> 2 mm; Temporary resistance: 640 - 940 MPa |
Calculated Properties Density: 7.86 g / cm3 |
Standard | Description |
---|---|
GOST 2246-70 |
Do not trust the content. The original aloro.org.