VZHL12U (VZHL12U-VI)
Production of cast bar stock for further refining during casting of blades and other shaped castings
Production of cast bar stock for further refining during casting of blades and other shaped castings
Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | V, % | Zr, % | Al, % | Pb, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | V, % | Zr, % | Al, % | Pb, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
OST 1-90126 - 85 | < 2 | < 0.4 | < 0.015 | < 0.0005 | < 0.4 | 12–15 | 8.5–10.5 | 4.2–4.7 | 53.8135–65.46 | 0.5–1 | < 0.02 | 5–5.7 | < 0.001 | < 0.02 | < 0.015 | 0.14–0.2 | < 0.015 | 0.5–1 | 2.7–3.4 | 1–1.8 |
Rolling | Standard | Size, mm | Tension | Classifiers | \sigma _{U}, MPa | \psi, % | d5, % | Treatment |
---|---|---|---|---|---|---|---|---|
Rolling | Standard | Size, mm | Tension | Classifiers | \sigma _{U}, MPa | \psi, % | d5, % | Treatment |
Workpiece | OST 1-90126 - 85 | 830 | 7 | 5 |
Standard | Treatment | Температура испытаний, ° С | Постоянно приложенное напряжение, МПа | Время до разрушения в часах, ч |
---|---|---|---|---|
Standard | Treatment | Температура испытаний, ° С | Постоянно приложенное напряжение, МПа | Время до разрушения в часах, ч |
OST 1-90126 - 85 | Without heat treatment | 975 | 200 | 40 |
Standard | Description |
---|---|
Standard | Description |
OST 1-90126 - 85 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Bi | % | Bismuth |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
V | % | Vanadium |
Zr | % | Zirconium |
Al | % | Aluminium |
Pb | % | Lead |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
W | % | Tungsten |
Do not trust the content. The original aloro.org.