Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Pb, % | P, % | C, % | S, % | O, % | Mo, % | N, % | W, % | Ta, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Pb, % | P, % | C, % | S, % | O, % | Mo, % | N, % | W, % | Ta, % |
UNS | < 1 | < 0.75 | 0.01–0.02 | < 5.0E-5 | < 1 | 9.5–10.5 | 18–21 | 2.75–3.25 | 43.85295–55.46 | 0.05–0.15 | 4.2–4.8 | < 0.002 | < 0.03 | 0.03–0.1 | < 0.03 | < 0.01 | 3.5–5 | < 0.005 | 5.5–6.5 | 1–2 |
Germany |
---|
Germany |
2.4654 (NiCr20Co13Mo4Ti3AI) |
Standard | Description |
---|---|
Standard | Description |
UNS |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Bi | % | Bismuth |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Ni | % | Nickel |
Zr | % | Zirconium |
Al | % | Aluminium |
Pb | % | Lead |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
O | % | Oxygen |
Mo | % | Molybdenum |
N | % | Nitrogen |
W | % | Tungsten |
Ta | % | Tantalum |